THREETEX™ Series
Polyester
| Pad-Steam Process | |
| THREETEX™ Series OBA | 1.0 ~ 10g/l |
| Dip and Squeeze | pick up 50 ~ 100% |
| High-temp steam | 150℃~ 170℃ |
| Developing time | 2 ~ 5min |
Application for polyester fibers
| Pad-Steam Process | |
| THREETEX™ Series OBA | 1.0 ~ 10g/l |
| Dip and Squeeze | pick up 50 ~ 100% |
| High-temp steam | 150℃~ 170℃ |
| Developing time | 2 ~ 5min |